Model Number : Alloy 90
Brand Name : Zhonggong Special Metallurgy
Place of Origin : China
MOQ : 100KG
Price : Price is negotiated based on the required specifications and quantity
Payment Terms : Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability : 5000 tons per month
Delivery Time : 5-8 working days, depending on the parameters required for negotiation
Packaging Details : Standard export packaging, or packaging as required
Composition : Nickel (Ni): 57-59%, Chromium (Cr): 13-15%, Iron (Fe): 13-15%, Cobalt (Co): 2.5-3.5%, Molybdenum (Mo): 2.5-3.5%, Tungsten (W): 1.5-2.5%, Titanium (Ti): 1.0-2.0%, Aluminum (Al): 1.0-2.0%
Application : Gas turbines, aerospace components, industrial processes
Density : 8.24 g/cm³
Tensile Strength : 760-1035 MPa
Yield Strength : 420-690 MPa
Modulus of Elasticity : 205-215 GPa
Thermal Conductivity : 11-13 W/(m·K)
Melting Point : Approximately 1320-1380°C
Corrosion Resistance : Excellent resistance to oxidation and high temperatures
Fatigue Resistance : High fatigue resistance
Creep Resistance : Excellent at elevated temperatures
Hardness : 28-35 HRC
Certification : ISO Certificate
Alloy 90: Advanced Nickel-Based Superalloy For High-Temperature Applications
Alloy 90 Product Description:
Alloy 90, a nickel-based superalloy, is engineered for high-performance applications requiring exceptional strength, heat resistance, and corrosion resistance. Composed primarily of nickel with significant additions of chromium, iron, cobalt, molybdenum, tungsten, titanium, and aluminum, this alloy exhibits outstanding mechanical properties at elevated temperatures.
Key Features:
Alloy 90 remains a cornerstone in industries demanding reliability, durability, and performance under demanding operational conditions, making it a preferred choice for critical components in aerospace and industrial sectors worldwide.
Here is a detailed composition table for Alloy 90:
Element | Weight Percentage (%) |
---|---|
Nickel (Ni) | 57-59 |
Chromium (Cr) | 13-15 |
Iron (Fe) | 13-15 |
Cobalt (Co) | 2.5-3.5 |
Molybdenum (Mo) | 2.5-3.5 |
Tungsten (W) | 1.5-2.5 |
Titanium (Ti) | 1.0-2.0 |
Aluminum (Al) | 1.0-2.0 |
![]() |